About the product
Star-shaped nanoparticles produced by chemical synthesis. The product is a colloidal system in aqueous solution stabilized with sodium citrate and is supplied as 0.5 mL of colloidal solution with a particle concentration of about 10⁹ mL⁻¹.
The anisotropic shape of the particles creates local regions of enhanced electromagnetic field, which makes such structures promising for surface-enhanced Raman scattering.
The particles tend to aggregate when stored for more than 4 hours, which should be taken into account when planning experiments.

Specifications
- Size
- 50–250 nm by DLS
- Concentration
- about 10⁹ particles per mL
- Stabilizer
- sodium citrate, aqueous medium
- Storage
- use within 4 hours of synthesis
request
We will tailor size, concentration and surface to your task
Other products
all products
Gold nanoparticles
Gold nanospheres
monodisperse, 15–150 nm
- Concentration
- 10⁹–10¹¹ particles per mL
- Stabilizer
- CTAC, aqueous medium
- lead time
- 2 days
Gold nanoparticles
Gold nanorods
resonance at 850–1100 nm
- Resonance
- longitudinal, 850–1100 nm
- Concentration
- about 10⁹ particles per mL
- lead time
- 1 day
Gold nanoparticles
Gold nanocubes
well-defined facets, 30–80 nm
- Concentration
- about 10¹¹ particles per mL
- Stabilizer
- CTAB, aqueous medium
- lead time
- 2 days